6. Adoption of Inconel Alloy 625 Cladding

来源:百度知道 编辑:UC知道 时间:2024/07/01 04:08:23
6. Adoption of Inconel Alloy 625 Cladding
Waterwall areas that are not protected by a refractory lining and the superheater tubes are the most corrosion prone areas. Cladding consists of overlaying a layer of Inconel 625 (21Cr-9Mo-3.5Nb-Ni base) on tubes to protect them from the attack of HCl/Cl2. This method has been used successfully in the waterwall tubes and part of the superheater tube bundles in many WTE facilities. The key element regarding the cost is how much Inconel 625 is used and where. Some researchers have shown that Inconel 625 applied on waterwall tubes provides excellent corrosion resistance . Although the price of Inconel 625 is higher than that of a protective refractory lining, the cost of Inconel 625 is partly compensated by avoiding the cost of refractory maintenance. In addition, Inconel 625 has higher thermal conductivity than refractory materials and therefore can reduce gas temperature in the first gaspass.
The application of Inconel 625 on superheat

6. Inconel合金625金属的收养
没有受加工困难的衬里和过热器管的保护的Waterwall地区是多数腐蚀有倾向的区域。 金属包括覆盖Inconel 625 (21Cr 9Mo 3.5NbNi层数在管的基地)保护他们免受HCl/Cl2攻击。 这个方法在过热器管捆绑的waterwall管和部分顺利地使用了在许多WTE设施的。 关于费用的关键字元是多少使用Inconel 625,并且的地方。 有些研究员表示,在waterwall管625申请的Inconel提供优秀耐腐蚀性。 虽然Inconel 625的价格高于那防护加工困难的衬里, Inconel 625的费用通过避免加工困难的维护的费用部分补偿。 另外, Inconel 625比耐火材料并且可能减少在第一gaspass的有更高的导热性气体温度。
因为金属的表现取决于在操作时,被到达的金属温度Inconel 625的应用在过热器管的是更加复杂的。 一项研究表示, Inconel 625不提供在400-420 C750-840 _F之上的防护)。 另一项研究表明在金属温度大约540 _C (1000年_F), Inconel 625的副产品率是0.2 lm/h (0.069英寸或年) (Ref 13)。 某些的锅炉现有的WTE设施被设计经营在低温并且可能申请在过热器管捆绑的Inconel 625。 然而,因为终身Inconel 625金属是变化莫测的,问题仍然出现。 它也许持续多达二年或者一样少许象三个月。 根据作者从WTE设施得到的数据,替换过热器管捆绑的费用用Inconel 625金属是$350,000/unit; 并且没有Inconel 625金属的仅$250,000/unit。 设施的人工成本是$75,000/unit。 如果过热器管捆绑的终身与Inconel 625金属的是十分地更长的,这金属的追加成本可以由管的停工和替换的被避免的费用补偿。 为新的WTE设施,锅炉被设计经营420 _C,过热器管金属